| Appearance | Transparent liquid | |
| Viscosity (Iwata - 2 cups) | 8.5-9.5 S | |
| UV component (%) | 35±2 % | |
| Density (g/cm³, 25ºC) | 0.90±0.05 | |
| Coating performance | ||
| Hardness (1Kg force load) | 2H-4H | |
| Coating thickness (μm) | 5-15 | |
| Boiling performance (surface spray paint, no primer 100ºC/60min) | Adhesion 5B, no change in coating | |
| Bending (cylindrical shaft diameter) | 40mm | |
| Curing energy (mercury lamp, mj/cm²) | 600-1,000 | |
| QUV resistance | More than 200h | |
| Anti-friction performance (1Kg load-bearing, wear-resistant machine, 1*1 grinding head, 0000# steel wool) | 50 times, no wear marks | |
| Anti-graffiti (Zebra oil-based pen) | General | |
| Water contact angle | General | |
| Note: The above performance parameters can be customized according to customer requirements | ||
Texture decoration and shell molding of mobile phones, laptops, home appliances and other products.
1. Clean the material surface.
2. Pour the glue into the metal mold, fit the PC or PET to the metal mold, and use a glue stick to squeeze the surface of the material so that the glue can expel air bubbles and achieve better leveling. Make sure that the bonding parts are covered with glue.
3. Irradiate with ultraviolet light with a wavelength of 265 or 395 nanometers. When irradiating, keep the UV lamp as close to the glue as possible to speed up the curing.
4. Tear off the PC or PET from the metal mold. At this time, the adhesive layer is completely peeled off and stuck to the surface of the PC or PET.
5. If the adhesive layer is not completely cured, you can continue to use UV light until the adhesive layer is fully cured.
Unwind → Glue on specially treated release film → Mold rolling → UV curing → Demold → Rewind → Printing ink, etc. → Cutting → Forming → Injection molding → Peel off the surface polyester film → Spray hardened layer
1. Ensure that the UV adhesive layer absorbs sufficient UV energy to achieve the best curing effect, otherwise it will easily affect the performance of the adhesive layer.